Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni – 19.5Cr – 13.5Co – 4.3Mo – 3.0Ti – 1.4Al – 0.05Zr – 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated

Published By Publication Date Number of Pages
SAE 2017-06-13 8
Guaranteed Safe Checkout
Categories: , ,

If you have any questions, feel free to reach out to our online customer service team by clicking on the bottom right corner. We’re here to assist you 24/7.
Email:[email protected]

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, flash welded rings, 3.25 inches (82.6 mm) and under and stock of any size for forging and for flash welded rings. (see 8.5).