D6604-00(2013) Standard Practice for Glass Transition Temperatures of Hydrocarbon Resins by Differential Scanning Calorimetry

Published By Publication Date Number of Pages
ASTM 2013 4
Guaranteed Safe Checkout
Categories: ,

If you have any questions, feel free to reach out to our online customer service team by clicking on the bottom right corner. We’re here to assist you 24/7.
Email:[email protected]

ASTM D6604-00-Reapproved2013

Historical Standard: Standard Practice for Glass Transition Temperatures of Hydrocarbon Resins by Differential Scanning Calorimetry

ASTM D6604

Scope

1.1 This practice covers determination of glass transition temperatures of hydrocarbon (HC) resins by differential scanning calorimetry (DSC).

1.2 This practice is applicable to HC resins as defined in Terminology D6640. The normal operating temperature range is from the cryogenic region to approximately 180°C. The temperature range can be extended.

1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.4 Further discussion of glass transition can be found in Test Method D3418, and Test Method E1356.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Keywords

DSC; glass transition temperatures; hydrocarbon resins; Tg

ICS Code

ICS Number Code 83.080.20 (Thermoplastic materials)

DOI: 10.1520/D6604-00R13

ASTM-D6604 2013
$35.75