BS IEC 61747-40-6:2018
$102.76
Liquid crystal display devices – Mechanical testing of display cover glass for mobile devices. Retained biaxial flexural strength (abraded ring-on-ring)
Published By | Publication Date | Number of Pages |
BSI | 2018 | 18 |
This part of IEC 61747 is a mechanical performance testing procedure for cover glass used in electronic flat panel displays in mobile devices. This document focuses on the measurement of surface fracture load after flaw introduction via grit particle abrasion. After abrasion, the retained surface fracture load is measured with the method documented in IEC 61747-40-4.
PDF Catalog
PDF Pages | PDF Title |
---|---|
2 | undefined |
4 | CONTENTS |
5 | FOREWORD |
7 | INTRODUCTION |
8 | 1 Scope 2 Normative references 3 Terms and definitions |
9 | 4 General |
10 | 5 Apparatus 5.1 Testing environment and pre-conditioning 5.2 Abrasion device |
11 | Figures Figure 1 – Abrasion device |
12 | 5.3 Abrasion material 5.4 Pressurization source 6 Procedure 6.1 Safety 6.1.1 Hazard – Broken glass 6.1.2 Hazard – Airborne particulate 6.2 Sample Figure 2 – Specimen holder |
13 | 6.3 Abrasion testing – Individual specimen 6.4 Complete the report 7 Retained failure load testing 8 Specifications |
14 | Annex A (informative) Check depth measurement Figure A.1 – Schematic of fracture surface with measurement of check depth Figure A.2 – Check depth measurement for grit particle abraded glass – Example 1 |
15 | Figure A.3 – Check depth measurement for grit particle abraded glass – Example 2 Figure A.4 –Check depth measurement for grit particle abraded glass – Example 3 |
16 | Figure A.5 –Check depth measurement for grit particle abraded glass – Example 4 |
17 | Bibliography |