BS ISO 19604:2018
$142.49
Fine ceramics (advanced ceramics, advanced technical ceramics). Mechanical properties of ceramic composites at high temperature. Determination of stress-rupture time diagram under constant tensile loading
Published By | Publication Date | Number of Pages |
BSI | 2018 | 28 |
This document specifies the conditions for determination of the stress-rupture time diagram of continuous fibre-reinforced ceramic matrix composites (including carbon fibre-reinforced carbon matrix composite) at high temperature in air, vacuum and inert gas atmospheres under constant tensile loading.
This document applies to all ceramic matrix composites with continuous fibre reinforcement: unidirectional (1D), bidirectional (2D) and tridirectional (xD, with 2 < x ≤ 3), loaded along one principal axis of reinforcement.
NOTE 1 In most cases, ceramic matrix composites to be used at high temperature in air are coated with an antioxidation coating.
NOTE 2 Since the main purpose of the test is to obtain the stress-rupture time data, the deformation measurement is not mandatory.
PDF Catalog
PDF Pages | PDF Title |
---|---|
2 | National foreword |
7 | Foreword |
9 | 1 Scope 2 Normative references 3 Terms, definitions and symbols |
11 | 4 Principle 5 Significance and use 6 Apparatus 6.1 Test machine |
12 | 6.2 Gripping devices 6.2.1 General 6.2.2 Active gripping devices 6.2.3 Passive gripping devices 6.3 Test chamber 6.4 Load indicator |
14 | 6.5 Extensometer 6.5.1 General |
15 | 6.5.2 Mechanical extensometer 6.5.3 Electronic optical extensometer 6.6 Heating apparatus 6.7 Temperature measurement devices |
16 | 6.8 Data recording system 6.9 Micrometers 7 Test specimens 7.1 Test specimen geometry |
17 | 7.2 End tabs of specimen |
18 | 7.3 Test specimen preparation |
19 | 7.4 Number of test specimens 8 Test preparation 8.1 Alignment adjustment in tensile axis direction 8.2 Adjustment of heating apparatus and temperature measuring device 8.3 Measurement of test specimen dimension |
20 | 9 Test procedures 9.1 Testing technique 9.1.1 Test specimen mounting 9.1.2 Setting of extensometers 9.1.3 Setting of inert atmosphere 9.1.4 Heating the test specimen |
21 | 9.1.5 Monitoring of temperature and elongation 9.1.6 Applying load 9.2 Post-testing treatment 9.3 Test validity |
22 | 9.4 Stress levels in tests 9.5 Accidental interruption of the test 10 Calculation of results 10.1 Tensile applied stress |
23 | 10.2 Tensile strain 10.3 Drawing of tensile strain curve 10.4 Drawing of stress-rupture diagram 11 Test report |
25 | Annex A (informative) Measurement procedure of bending ratio in the adjustment of a tensile axis |